Lamellar tearing - useful information for candidates attending NDT Training


*In general occurs beneath the T-joint welds
*can be observed in thick plates with poor through-thickness ductility
*Usually occurs in large welds
*Welding heats the steel and it expands and while cooling “Tears” the steel